Hafnium Metal Hf 99.9% High Purity for Nuclear Control Rods, Superalloys and Plasma Cutting Components
US$3,100.00
1 kg

Product profile

Customization

Available

Product name

Hafnium Metal

CAS No

7440-58-6

Model NO.

ET-HfM-01

EINECS No

231-166-4

Density

13.31 G/cm³

Melting Point

2227°C

Boiling Point

4602°C

Transport Package

Cardboard Boxes or Barrels

Specification

50kg per barrel

Trademark

Eternal-Element

Origin

China

Key features

99.9% High Purity
High Neutron Absorption Capability
Suitable for Nuclear Control Rods
Suitable for Nickel Based Superalloys
Suitable for Plasma Cutting Components

Company profile

Shanghai Sheeny Metal Mateirals Co., Ltd.
Exhibition ExperienceYears of Export ExperienceHigh Repeat Buyers ChoiceImporters and Exporters
Business Type: Trading CompanyAverage Response Time: ≤0.38h

About Our Factory & Business Background

AddressRoom 310, Building 1, No. 326 Jinyuan 3rd Road, Jiading District, Shanghai, China
Average Lead TimePeak Season Lead Time: 1-3 months Off Season Lead Time: 1-3 months

Our Production Capability & Technical Expertise

Main ProductsErbium Oxide, Holmium Oxide, Thulium Oxide, Ytterbium Oxide, Lutetium Oxide, Yttrium Oxide, Scandium Oxide, Hafnium Oxide, Tantalum Oxide, Germanium Oxide

Our Industry Experience & Global Business Record

Main MarketsNorth America, Western Europe, Eastern Asia

Product Q&A

Q:Why should I choose your company as my rare earth materials supplier?
A:
We are a professional supplier specializing in high-purity rare earth materials and advanced metal materials. With extensive industry experience, reliable supply capabilities and strict quality control, we provide stable and trusted material solutions for global customers.
Q:What types of rare earth materials do you supply?
A:
We are a professional supplier specializing in high-purity rare earth materials and advanced metal materials. With extensive industry experience, reliable supply capabilities and strict quality control, we provide stable and trusted material solutions for global customers.
Q:How do you ensure product quality?
A:
We provide a wide range of rare earth products, including rare earth metals, oxides, salts, alloys and other customized advanced materials. Different purities, specifications and product forms are available according to customer requirements.
Q:Can you provide customized products according to our requirements?
A:
We provide a wide range of rare earth products, including rare earth metals, oxides, salts, alloys and other customized advanced materials. Different purities, specifications and product forms are available according to customer requirements.
Q:Do you have the capability to supply large-volume orders?
A:
We provide a wide range of rare earth products, including rare earth metals, oxides, salts, alloys and other customized advanced materials. Different purities, specifications and product forms are available according to customer requirements.

Send Inquiry

*To:Shanghai Sheeny Metal Mateirals Co., Ltd.Shanghai Sheeny Metal Mateirals Co., Ltd.
*Content:
0/4000

Supplier replies will be sent to your registered email

You may also like

Premium High Purity Silicon Metal for Industrial Use
Made-in-China.com
High Purity Silicon Metal 553 Lump for Industry
Made-in-China.com
Premium High Purity Strontium Metal for Global Distribution
Made-in-China.com