SourcingAI
Try for free
Powered by Made-in-China.com
High Quality Machine Grade LLDPE Stretch Wrap Film Featuring 400% Stretch Rate
US$7.50
1-999 Rolls
US$7.40
1,000-4,999 Rolls
US$7.30
5,000+ Rolls

Product specifications

Thickness

Width

Length

Sample price:US$8.00/roll.Request sample

Product profile

Customization

Available

Material

PE

Usage

Packaging Film, Agriculture

Model NO.

GUANFU301

Processing Type

Blow Molding

Transparency

Transparent

Feature

Moisture Proof

Color

Customized Color

Logo

Accept Customized Logo

Sample

Samples Offered

Delivery Time

7-15 Days

Size

Custom Size Accepted

Transport Package

Film Roll Packed by Woven Bag / Pallet

Specification

Model GF202, LLDPE Stretch Film,

Trademark

Guanfu

Origin

Shandong

HS Code

3901902000

Production Capacity

12000 Tons

Key features

High stretch-recovery performance::hand-use version 200%-400% elongation, machine-use version 300%-500% elongation. Metallocene option available for heavy-duty cargo.
Excellent inter-layer self-adhesion, no extra tape required.
Great puncture & tear resistance, provides dust-proof and moisture-proof protection.
High transparency for convenient cargo visual inspection without unpacking.
Two types for different operations:hand-use for manual small-lot wrapping:machine-use supports high-speed wrapping of 15-18 pallets per hour for mass production.
Multiple optional thickness and width sizes, widely applied in logistics, export, hardware, building materials and warehouse storage.

Company profile

Shandong Guanfu Plastic Industry Co., Ltd.
High Repeat Buyers ChoiceExperienced TeamFast DeliveryRaw-Materials Traceability
CertifiedBusiness Type: Trading Company CertifiedR&D Capacity: ODM Service Available CertifiedCustomization Options: Customization from Samples, Customization from Designs, etc. CertifiedExport Year: 1 yearNearest Port: Qingdao Port, Tianjin Port, Lianyungang PortAverage Response Time: ≤4.57h

About Our Factory & Business Background

AddressXiaoshan Congguixuan, South Section Huanghe Street, Zhengyang Road, Ningjin Town, Dezhou, Shandong, China
Plant Area134.5 square meters
Number of Employees12
Registered Capital5,000,000 RMB
Terms of PaymentLC, T/T, D/P, PayPal, Western Union, Small-amount payment, Money Gram
International Commercial Terms(Incoterms)FOB, EXW, CIF, CFR, DDP, DAT, FAS, DAP, CIP, CPT
Average Lead TimePeak Season Lead Time: within 15 workdays Off Season Lead Time: within 15 workdays
Minimum Order Quantity1 tons
Supply Chain Partners6

Our Production Capability & Technical Expertise

Main ProductsStretch Film, Silage Film, Bale Wrap Net
QA/QC inspectors1 people
Inspection Type for Finished ProductsRandom inspection(Function inspection)
Inspection Method for Finished ProductsHave instruction but no written records
R&D Engineers1 people
Traceability of Raw MaterialsYes

Our Industry Experience & Global Business Record

Year of Establishment2026-03-13
Main MarketsSouth America, North America, Eastern Europe, Western Europe
Repeat Buyers Choice80%~100%
Number of Foreign Trading Staff9
Overseas Agent/BranchNo
New Products Launched in Last yearNo

Our Certifications, Standards & Industry Recognition

Cooperated with Fortune 500No

Product Q&A

Q:What is the difference between PE stretch film and metallocene stretch film?
A:
Standard PE stretch film offers cost-effective general-purpose performance. Metallocene grade provides higher tensile strength and better puncture resistance for heavy-duty cargo packaging.
Q:Can stretch film work for outdoor long time storage of pallet goods?
A:
It can provide dust proof and moisture proof protection. For long term outdoor exposure, extra UV resistant treatment is recommended.
Q:Does your stretch film leave sticky residue on goods after removal?
A:
Our stretch film features inter layer self adhesion. It sticks to itself instead of cargo surfaces, so almost no residue will be left on packaged items.
Q:Can stretch film be used together with your silage film or bale net wrap for combined export orders?
A:
Sure. We support mixed container loading. Stretch film can wrap pallets of silage film and bale net wrap to secure whole container shipments.
Q:What elongation rates can your stretch film reach?
A:
Hand use stretch film reaches 200-400 percent elongation while machine use stretch film can hit 300-500 percent elongation.