Customized Precision Investment Casting Stainless Steel/Superalloy Casting Services
US$20.00
100-499 Pieces
US$18.00
500+ Pieces

Product specifications

Materials

Sample price:US$100.00/piece.Request sample

Product profile

Customization

Available

Casting Method

Thermal Gravity Casting

Process

Lost Wax Casting

Model NO.

HDCI093

Molding Technics

Pressure Casting

Application

as Per Customers Requirements

Material

Stainless Steel

Surface Preparation

Polishing

Surface Roughness

Ra12.5

Machining Tolerance

+/-0.10mm

Standard

AISI

Certification

CE, RoHS, ISO 9001:2000, ISO 9001:2008

Condition

New

Custom

Acceptable

After-Sales Service

Yes

Warranty

1 Year

MOQ

100

Lead Time

25-30 Days

Sample

Available

Transport Package

Cartons

Specification

As your request

Trademark

OEM

Origin

China

Production Capacity

800 Tons/Year

Company profile

Wuxi Henderchan Industrial Co Ltd
Customization from SamplesCustomization from DesignsFull CustomizationFlexible Customization
Business Type: Manufacturer/Factory, Trading Company CertifiedR&D Capacity: ODM Service Available & OEM Service Available CertifiedCustomization Options: Customization from Samples, Customization from Designs, etc. CertifiedExport Year: 9 Years CertifiedNearest Port: Shanghai PortAverage Response Time: ≤3.04h

About Our Factory & Business Background

AddressUnit 1, Jiangda Kejiyuan, No. 99, Jinxi Road, Wuxi, Jiangsu, China
Terms of PaymentLC, T/T, D/P, PayPal, Western Union, Small-amount payment
International Commercial Terms(Incoterms)FOB, CIF, CFR, EXW
Average Lead TimePeak Season Lead Time: 1-3 months Off Season Lead Time: one month
Minimum Order Quantity50 Pieces
Supply Chain Partners20

Our Production Capability & Technical Expertise

Main ProductsCustom CNC Machining Parts, CNC Machining Service, Custom Investment Casting Parts, Investment Casting Service, Precision Forging Service, Custom Precision Forging Parts, Hinges, Go Kart Parts, Metal Fabrication Service, Custom Metal Fabrication Parts
R&D Engineers1 people

Our Industry Experience & Global Business Record

Year of Establishment2015-09-24
Main MarketsEurope
Repeat Buyers Choice80%~100%
Number of Foreign Trading Staff4
Overseas Agent/BranchNo
New Products Launched in Last yearNo

Send Inquiry

*To:Wuxi Henderchan Industrial Co LtdWuxi Henderchan Industrial Co Ltd
*Content:
0/4000

Supplier replies will be sent to your registered email

You may also like

Precision Stainless Steel Casting Services
Made-in-China.com