Product profile
Customization
AvailableCertification
CE, ISOPlace Style
VerticalRange of Applications
IndustrialType
Atomization EquipmentUsage
Metal Powder Pulverizing EquipmentFuel
ElectricModel No.
Kd-100Power Type
AC/380V/50HzMelting Furnace Power(Kw)
160Tundish Power(Kw)
15-45Gas Flow (L/Min)
8000-30000Medium Frequency Power Supply
IGBT:KgpsControl Method
Industrial Computer, PLCHS
8514199000Melting Temperature(℃)
1750Tundish Heating Method
Medium Frequency Induction / Resistance HeatingTemperature Measurement
Infrared Temperature Measurement/W/Re 5/26Cooling Method
Cooling Tower / Water Cooling Unit + Heat ExchangHMI
Analog Screen; Computer Touch ScreenProductioncapacity
100Transport Package
International StandardSpecification
KD-100Trademark
KEDA Induction FurnaceOrigin
Anhui HefeiHS Code
851420009Key features
High-Purity Powder Production: Vacuum or inert atmosphere prevents oxidation and impurities for high chemical purity.
Excellent Powder Morphology: Produces spherical powder with high sphericity, smooth surface, and minimal satellite particles.
Uniform Composition Control: Vacuum melting ensures homogeneous alloy composition suitable for reactive metals like Ti.
Adjustable Particle Size: Particle size distribution is controllable via gas pressure and metal flow rate adjustments.
Full Automation & Safety: PLC/computer control with multiple safety interlocks for reliable and safe operation.
Energy Efficient Design: Full-bridge IGBT series resonant design ensures high reliability and low specific power consumption.
Flexible Customization: Offers full, minor, and flexible customization from samples or designs.
Professional Packaging: Anti-rust treatment, moisture-proof bags, and sturdy plywood cases ensure safe transit.
Company profile

CertifiedBusiness Type: Manufacturer/Factory & Trading Company CertifiedR&D Capacity: ODM Service Available & OEM Service Available CertifiedCustomization Options: Customization from Samples, Customization from Designs, etc. CertifiedExport Year: 1 Year CertifiedNearest Port: Shanghai PortAverage Response Time: ≤15h
AI-Powered supplier vetting
SummaryThe supplier operates in technical services, electronic component manufacturing, special metallurgical equipment, and furnace-related manufacturing and sales. It reports ISO9001:2015 certification, inventory capability, broad customization options, and OEM service for well-known brands. However, it has no written corrective-action or complaint-handling procedures, no valid manufacturing-capacity contract with an affiliated subcontractor, no overseas warehouse, branch, agent, showroom, or stated overseas service country, and no recent fire-drill or factory environmental-impact assessment evidence. Financial information is inconsistent across the provided records and therefore cannot substantiate financial strength. The supplier has seven R&D engineers but no available SDK, and customer-case evidence is limited to OEM service without Fortune 500 cooperation.
Supplier typeThe supplier’s stated business scope covers technical services, electronic component manufacturing, special metallurgical equipment, ovens, furnaces, electric furnaces, related sales, and import/export activities. This supports classification as a manufacturer and technical equipment supplier rather than a pure trading company.
CertificationsThe supplier reports an ISO9001:2015 certificate in both its sustainable-development and management-system records. This is explicit certification evidence, although the slices do not provide certificate validity dates or scope details.
After-Sales capabilityAfter-sales controls are weakly documented: there are no written corrective/preventive-action procedures or complaint-handling records. The supplier has inventory capability, but no overseas warehouse, showroom, agent, branch, or stated overseas service coverage, limiting demonstrated international service support.
Production capacityThe business scope explicitly includes manufacturing electronic components, special metallurgical equipment, ovens, furnaces, and electric furnaces, and the supplier reports in-stock capability. However, there is no valid manufacturing-capacity contract with an affiliated subcontractor, which creates a documented capacity-governance deficiency.
Customization capabilityThe supplier explicitly offers customization from samples, designs, full customization, minor customization, and flexible customization. This is direct evidence of broad customization coverage.
Product Q&A
Q:What are the specific cost responsibilities of both parties regarding logistics and transportation?
A:
Under standard terms, our company is responsible for all freight, insurance, and related logistics costs to deliver the goods to the designated destination port (e.g., Shanghai Port). All costs incurred after the goods arrive at the destination port, including but not limited to port charges, import customs clearance fees, duties, taxes, and inland transportation to the final destination, are to be borne by the customer. For specific projects or special requirements, we offer flexibility. Altern
Q:How is the equipment packaged for shipment?
A:
To ensure safe transit, we employ robust packaging. This includes professional anti-rust treatment for precision surfaces, protection of protruding components with custom covers, securing doors with internal supports to prevent deformation, and final packaging in sealed moisture-proof bags within sturdy plywood cases.
Q:What are the delivery lead times?
A:
Standard lead times vary based on the product model and order volume. Please contact our sales team for a specific project schedule. We are committed to meeting agreed-upon delivery dates.
Q:What is the process for placing an order?
A:
The process typically involves: 1) Receiving your official Purchase Order (PO). 2) Issuing a Proforma Invoice (PI) for your review. 3) Upon your confirmation and advance payment as per the PI, we will schedule the production and delivery.
Q:What payment terms do you offer?
A:
We commonly operate on a T/T (Telegraphic Transfer) basis. Standard terms involve an advance payment to initiate the order, with the balance due before shipment. Other terms may be negotiable for large projects.
Send Inquiry
*To:
Hefei Keda Industrial Equipment Co., Ltd.
Hefei Keda Industrial Equipment Co., Ltd.*Content:
Supplier replies will be sent to your registered email
You may also like
High-Vacuum Induction Melting Furnace for Superalloy Development
US$35,000.00-100,000.00
1 Set(MOQ)
Vim Vacuum Induction Melting Furnace Solution for Aerospace Superalloys
US$1.00
1 Piece(MOQ)
Vacuum Induction Furnace for High-Purity Superalloys, Precious Metals, and Electronic-Grade Materials.
US$50,000.00-150,000.00
1 Set(MOQ)
Vacuum Induction Melting Furnace Manufacturers for High-Purity Superalloys, Rare Metals and Precious-Metal Ingots
US$50,000.00-150,000.00
1 Set(MOQ)
Induction Furnace for Superalloy Melting and Vacuum Casting
US$35,000.00-100,000.00
1 Set(MOQ)
High Power Density Induction Vacuum Degassing Furnace for Fast Melting
US$100,000.00-400,000.00
1 Piece(MOQ)
Vacuum Induction Melting Furnace for Non-Ferrous Metal
US$10,000.00-500,000.00
1 Piece(MOQ)
Industrial Induction Melting Furnace for Nickel, Cobalt, Iron-Based Superalloys and High-Alloy Steels
US$50,000.00-150,000.00
1 Set(MOQ)
Aps Induction Vacuum Electric Iron Alloy Melting Furnace for Making High Quality Steel Factory Price
US$200,000.00-290,000.00
1 Set(MOQ)
High Vacuum Induction Melting Furnace for Metal Melting in Industry
US$6,039.00-9,999.00
1 Set(MOQ)
Large Capacity Vacuum Induction Melting Furnace for Foundry Factory
US$4,300.00-6,500.00
1 Set(MOQ)
Vertical Aps China Smelting for Steel Vacuum Induction Melting Furnace with CE New
US$200,000.00-290,000.00
1 Set(MOQ)
Vacuum Induction Furnace Melting 10kg Price for Magnesium Silicon
US$20,000.00
1 Piece(MOQ)
Lab-Use Small Vacuum Induction Melting Furnace for Ingot Sample
US$50,000.00-150,000.00
1 Set(MOQ)
Vacuum Crucible Induction Melting Furnace for Materials
US$10,000.00
1 Piece(MOQ)
500kg Vacuum Industry Electric Induction Iron Melting Furnace for Steel
US$2,600.00
1 Set(MOQ)
Factory Price Aps Steel Molding China Induction for Brass Vacuum Melting Furnace
US$200,000.00-290,000.00
1 Set(MOQ)
Vacuum Induction Gold Melting Electric Furnace for Metal Casting and Steel Melting Industry Induction Furnace
US$3,069.00-6,500.00
1 Set(MOQ)
30-250kg Vacuum Induction Melting Furnace for Wax Casting and Investment Casting
US$159,999.00-499,999.00
1 Piece(MOQ)