Reduce Casting Defects Foundry Sand Binder Casting Bonding Clay Bentonite
US$130.00
1-4 Tons
US$100.00
5-9 Tons
US$65.00
10+ Tons
Sample price:US$0.00/piece.Request sample
Product profile
Customization
AvailablePackaging
25kg Per Woven BagColor
Light Yellow/GrayModel NO.
HHS-60Usage
Ceramic, Paper, Concrete, ModelShape
PowderViscosity
60-70/80-90Rheoplasticity Ratio
≤1.5PA/(MPa·S)Loss on Filtration
≤15.0ml75μm Sieve Residue
≤4Moisture
≤10%Sample
Can ProvideProduct Name
Casting BentoniteTransport Package
WovenSpecification
25kg/bag, 50kg/bag, CustomizedOrigin
ChinaProduction Capacity
200000 Ton/YearKey features
High Wet Compressive Strength: Provides sufficient wet strength to prevent sand mold deformation during transportation and boxing.
Excellent Thermal Stability: Prevents defects like sand flushing and inclusion under high-temperature molten metal pouring.
Superior Reusability: Low dead clay formation rate significantly reduces per-unit bentonite consumption.
Reduced Casting Defects: Improves surface smoothness and reduces scrap rates through precise selection and modification.
Breathability & Easy Shake-out: Proper particle size ensures permeability and easy collapse after pouring for cleaning.
Flexible Packaging Options: Available in 25kg woven bags or 1-ton ton bags to save handling costs and increase efficiency.
15+ Years Industry Experience: Deep technical accumulation and stable exports to over 60 countries and regions worldwide.
Source Manufacturer: Owns mining areas and modern production bases with full chain quality control from mining to processing.
Company profile
Business Type: Trading Company CertifiedR&D Capacity: ODM Service Available & OEM Service AvailableExport Year: 2020-05-01Nearest Port: Dalian Port, Tianjin Port, Jinzhou PortAverage Response Time: ≤4.71hTerms of Payment: LC, T/T, PayPal, etc.
AI-Powered supplier vetting
SummaryThe supplier is identified as a professional technical bentonite supplier with crushing, drying, grinding, and activation capabilities, more than 10 production lines, and stated annual output of 1,200,000 tons. It offers OEM, ODM, and limited customization services, but does not provide 3D software design, SDKs, or evidence of new products in the past year. Quality assurance is reported, while supplier approval, corrective-action, and complaint-handling procedures lack documented records. Overseas service coverage is limited: no overseas showroom, agents, branches, or offline trade-show participation are reported. RoHS is the only stated certification. Financial information is incomplete and largely represented by placeholder values, so financial credibility cannot be reliably assessed. No specific customer cases are provided.
Supplier typeThe supplier explicitly identifies as a professional technical supplier and describes bentonite production using crushing, drying, grinding, and activation technologies. Its factory information indicates more than 10 production lines and production focused on bentonite.
CertificationsRoHS is explicitly listed as the supplier’s sustainable-development and product-certification capability. No other certifications are provided in the supplied information.
Production capacityThe supplier reports more than 10 production lines, 6–10 quality-control staff, bentonite output of 1,200,000 tons, and infrastructure including production facilities and a quality-assurance laboratory. These data explicitly support substantial production capacity, although the stated capacity figures are not fully consistent across the slices.
Customization capabilityThe supplier provides minor customization and customization from customer designs, and explicitly offers ODM and OEM services for popular brands. This supports a clear ability to adapt or manufacture according to customer requirements, though 3D software design and SDK support are unavailable.
Product Q&A
Q:What are the main components of bentonite?
A:
The main component of bentonite is montmorillonite, which is a natural silicate clay mineral. The higher the content of montmorillonite, the better the bonding, adsorption, and swelling properties of bentonite.
Q:Are you a production factory or a trading company? How to ensure product quality?
A:
We are a source manufacturer with self operated mining areas and modern production bases, achieving full chain quality control from mining to processing. All of our products have undergone strict laboratory testing, and we also support you in sending samples to any institution you specify for retesting. We have absolute confidence in the quality of our products.
Q:How do you view the future development trend of the bentonite industry?
A:
We believe that the industry is developing towards three directions: refinement, functionalization, and environmental protection.
Q:I am a beginner and unsure which type of bentonite to choose. Can you provide any advice?
A:
Of course you can! Please tell us your specific application areas (such as drilling, casting, feed, mud making, etc.)
Q:How long have you been in this industry? What markets are primarily served?
A:
We have been deeply involved in the bentonite industry for over 15 years, with rich production experience and profound technical accumulation. Our products not only hold a significant market share in the domestic market, but also have stable exports to over 60 countries and regions worldwide, including Southeast Asia, the Middle East, Europe, and South America. We have established long-term cooperative relationships with numerous drilling companies, foundries, and environmental engineering enter
Send Inquiry
*To:
Pureytech Materials (Shenyang) Co., Ltd
Pureytech Materials (Shenyang) Co., Ltd*Content:
Supplier replies will be sent to your registered email
You may also like
High Quality Efficient Multifunctional Foundry Sand Bonding Bentonite for Complex Precision Casting
US$70.00-210.00
1 Ton(MOQ)
Casting Mold Strength Reduce Defects Sand Casting Bonding Clay Bentonite
US$65.00-130.00
1 Ton(MOQ)
Green Sand Molding Casting Bonding Clay Foundry Reduce Casting Defects Bentonite
US$65.00-130.00
1 Ton(MOQ)
Green Sand Calcium Foundry Grade Additives Casting Bonding Clay Bentonite for Steel
US$65.00-130.00
1 Ton(MOQ)
Foundry Grade Green Sand Additives Low Dust Bentonite Clay for Casting
US$65.00-130.00
1 Ton(MOQ)
High Quality Sodium Bentonite for Foundry Molding Sand Bonding
US$70.00-210.00
1 Ton(MOQ)
Foundry Grade Bentonite for Sand Casting Binding
US$130.00-136.00
25 Tons(MOQ)
Premium Sodium Bentonite Clay for Foundry & Casting Supplies
US$200.00-350.00
1 Ton(MOQ)
Premium Calcium Bentonite Clay for Enhanced Foundry Sand Performance
US$210.00-220.00
7 Tons(MOQ)
Sustainable Bentonite Clay Solutions for Industrial Metal Casting
US$200.00-350.00
1 Ton(MOQ)
High Purity Bentonite Powder for Foundry Sand - Strong Bonding & Mold Stability
US$150.00-300.00
1 Ton(MOQ)
Premium Organic Bentonite Clay for Industrial Binder Applications
US$200.00-350.00
1 Ton(MOQ)
Sodium-Based Bentonite Clay Used as Filler for Foundry and Drilling Mud
US$500.00-1,000.00
1 Ton(MOQ)
Bentonite for Animal Nutrition and Feed Binder Use
US$150.00-300.00
1 Ton(MOQ)
Low Impurity Bentonite Powder for Iron Casting
US$130.00-136.00
25 Tons(MOQ)