High Accuracy Laboratory Concrete Creep Testing Rig Creep Deformation Test Machine
US$9,000.00
1-49 Pieces
US$6,000.00
50+ Pieces

Product profile

Customization

Available

After-sales Service

Yes

Warranty

One-year

Model NO.

TBTXBJ Series

Capacity

500KN/1000KN

Measurement range

0-500KN/0-1000KN

Relative reading error

±1%

Spring height

300mm

Spring compression stroke

52mm

Thickness of platen

50mm/70mm

Diameter of screw rod

52mm

Size of big platen

620mm/800mm

Size of small platen

520mm/600mm

Transport Package

Standard Export Packing

Specification

ISO

Trademark

TBT

Origin

Nanjing, China

HS Code

90158790

Production Capacity

50sets/Month

Key features

Dual Capacity Options: Available in 500KN and 1000KN capacities to suit various testing needs.
Customizable Dimensions: Spring stroke and compression space can be adjusted according to customer requirements.
Durable Construction: Platens and columns made of No.45 Steel with CNC machining for high durability.
Versatile Sample Support: Main frame suitable for 3pcs D150 x H300 mm concrete cylindrical samples.
Flexible Pump System: Comes with hand hydraulic pump; electric pump system available as optional configuration.
One-Year Warranty: Comes with a one-year warranty and after-sales service support.

Company profile

Nanjing T-Bota Scietech Instruments & Equipment Co., Ltd.
Importers and ExportersHigh Repeat Buyers ChoiceYears of Export ExperienceExperienced Team
Business Type: Manufacturer/Factory, Trading CompanyExport Year: 2008-01-02Nearest Port: SHANGHAIAverage Response Time: ≤4.51hTerms of Payment: LC, T/T, D/P, etc.International Commercial Terms(Incoterms): FOB, CFR, CIF, FAS, DDP, DAP, CIP, CPT, FCA, EXW

About Our Factory & Business Background

AddressRoom 1001, Huaxia Mansion, No. 81, Zhongshan Rd, Nanjing, Jiangsu, China
Average Lead TimePeak Season Lead Time: within 15 workdays Off Season Lead Time: within 15 workdays

Our Production Capability & Technical Expertise

Main ProductsUniversal Testing Machine, Compression Testing Machine, Soil Testing Instruments, Petrolium Testing Machine, Geo-Technical Testing Machine, Surveying Testing Machine, Non-Destructive Testing Machine, Asphalt&Pavement Testing Machine, Concrete&Cement Testing Machine, Lab Equipment

Our Industry Experience & Global Business Record

Main MarketsNorth America, South America, Eastern Europe, Southeast Asia, Africa, Oceania, Mid East, Eastern Asia, Western Europe

Product Q&A

Q:How long is the delivery time?
A:
Normally goods will be shipped out within 7-10days after contract signed and down payment received.
Q:Is it possible to make our own brand/logo on your product?
A:
Yes, but depends on MOQ.
Q:What's your MOQ?
A:
This depends on different types of products. If it is a large machine, the MOQ is usually 1 set. For small instruments, such as thermometers, the MOQ is 50 pieces.
Q:What kind of payment term you accept?
A:
Normally, 1) If total contract value less than USD 10,000.00 : 100% T/T in advance after contract signed. 2) If total contract value more than USD 10000.00 : 50% T/T in advance after contract signed and 50% T/T after receipt of BL copy. Or, irrevocable LC is acceptable

Send Inquiry

*To:Nanjing T-Bota Scietech Instruments & Equipment Co., Ltd.Nanjing T-Bota Scietech Instruments & Equipment Co., Ltd.
*Content:
0/4000

Supplier replies will be sent to your registered email

You may also like