SourcingAI
Try for free
Powered by Made-in-China.com
Superalloy Pipe Heat Resistant Nickel Based Industrial Tube
US$15.00-45.00
100 kg

Product specifications

Material

Sample price:US$2.50/kg.Request sample

Product profile

Customization

Available

After-sales Service

After-Sales Support Included

Warranty

12 Months

Model NO.

625/718/800/800H/825

Type

Seamless

Technique

Hot Rolled

Material

Alloy Steel

Surface Treatment

Polished

Usage

Boiler Pipe, Oil/Gas Drilling, Chemical Industry, Special Purpose

Section Shape

Round

Width

Customizable

Thickness

Customizable

Length

Customizable

Size

Customizable

Transport Package

Sea Freight Packaging

Specification

2000-4000mm or customizable

Trademark

jiangsuzunxiang

Origin

China

HS Code

7507120000

Production Capacity

50000

Key features

Customizable Dimensions: Width, thickness, length, and size are fully customizable to meet specific requirements.
Wide Material Range: Available in Nickel 200, Monel 400, Inconel 625, Hastelloy C276, and other superalloys.
Comprehensive Quality Testing: Includes PMI, tensile, hardness, bending, ultrasonic, and pressure testing for all pipes.
Diverse Surface Finishes: Offers pickled, polished, 2D, No. 4, No. 6, and No. 7 finishes based on client needs.
12 Months Warranty: Provides a one-year warranty period for all purchased industrial tubes.
Fast Delivery Time: Standard delivery within 7-15 days after order confirmation.
OEM and ODM Services: Full customization available including production from samples and drawings.
Global Sample Shipping: Samples can be sent to any location worldwide upon request.

Company profile

Importers and ExportersHigh Repeat Buyers ChoiceExperienced TeamCustomization from Samples
CertifiedBusiness Type: Trading Company CertifiedR&D Capacity: ODM Service Available & OEM Service Available CertifiedCustomization Options: Customization from Samples, Full Customization, etc. CertifiedExport Year: 1 Years CertifiedNearest Port: Qingdao / Tianjin PortAverage Response Time: ≤1.08h

About Our Factory & Business Background

AddressWuxi, Jiangsu, China
Plant Area60 square meters
Number of Employees6
Registered Capital10,000,000 RMB
Terms of PaymentLC, T/T, D/P, PayPal, Western Union, Small-amount payment
International Commercial Terms(Incoterms)FOB, CIF, CFR, EXW
Average Lead TimePeak Season Lead Time: one month Off Season Lead Time: one month
Minimum Order Quantity100 Kg
Supply Chain Partners20

Our Production Capability & Technical Expertise

Main ProductsStainless steel pipe, stainless steel elbow, stainless steel bar, stainless steel strip,alloy pipe alloy bar, alloy plate
R&D Engineers1 people

Our Industry Experience & Global Business Record

Year of Establishment2025-07-24
Main MarketsSouth America
Repeat Buyers Choice50%~80%
Number of Foreign Trading Staff5
Overseas Agent/BranchNo
New Products Launched in Last yearNo

Our Certifications, Standards & Industry Recognition

Cooperated with Fortune 500No

Product Q&A

Q:Can you send samples?
A:
Of course, we can send samples to all parts of the world.
Q:What are the shipping ports?
A:
Under normal circumstances, we ship from Tianjin, Qingdao ports, you can choose other ports according to your needs.
Q:What are the certifications for your products?
A:
We have ISO 9001, SGS, EWC and other certifications.
Q:How long does your delivery time take?
A:
In general, our delivery time is within 7-15 days, and may be delayed if the demand is extremely large or special circumstances occur.
Q:Can I go to your factory to visit?
A:
Of course, we welcome customers from all over the world to visit our factory.

Send Inquiry

*To:Jiangsu Zunxiang International Trade Co., Ltd.
*Content:
0/4000

Supplier replies will be sent to your registered email

You may also like