SourcingAI
Try for free
Powered by Made-in-China.com
High Temp Resistant Inconel Nickel Based Superalloy Seamless Pipe
US$30.00-45.00
100 kg

Product specifications

Material

Sample price:US$2.50/kg.Request sample

Product profile

Customization

Available

After-sales Service

After-Sales Support Included

Warranty

12 Months

Model NO.

600/601/625/690/718/X-750

Type

Seamless

Technique

Hot Rolled

Material

Alloy Steel

Surface Treatment

Polished

Usage

Boiler Pipe, Oil/Gas Drilling, Chemical Industry, Special Purpose

Section Shape

Round

Width

Customizable

Thickness

Customizable

Length

Customizable

Size

Customizable

Transport Package

Sea Freight Packaging

Specification

2000-4000mm or customizable

Trademark

jiangsuzunxiang

Origin

China

HS Code

7507120000

Production Capacity

50000

Key features

Superior corrosion resistance in harsh chemical and marine environments
Precise dimensional tolerance, stable mechanical properties for industrial applications
Excellent corrosion resistance against acid, alkali and seawater media
Stable mechanical properties with precise size consistency for industrial processing

Company profile

Importers and ExportersHigh Repeat Buyers ChoiceExperienced TeamCustomization from Samples
CertifiedBusiness Type: Trading Company CertifiedR&D Capacity: ODM Service Available & OEM Service Available CertifiedCustomization Options: Customization from Samples, Full Customization, etc. CertifiedExport Year: 1 Years CertifiedNearest Port: Qingdao / Tianjin PortAverage Response Time: ≤1.08h

About Our Factory & Business Background

AddressWuxi, Jiangsu, China
Plant Area60 square meters
Number of Employees6
Registered Capital10,000,000 RMB
Terms of PaymentLC, T/T, D/P, PayPal, Western Union, Small-amount payment
International Commercial Terms(Incoterms)FOB, CIF, CFR, EXW
Average Lead TimePeak Season Lead Time: one month Off Season Lead Time: one month
Minimum Order Quantity100 Kg
Supply Chain Partners20

Our Production Capability & Technical Expertise

Main ProductsStainless steel pipe, stainless steel elbow, stainless steel bar, stainless steel strip,alloy pipe alloy bar, alloy plate
R&D Engineers1 people

Our Industry Experience & Global Business Record

Year of Establishment2025-07-24
Main MarketsSouth America
Repeat Buyers Choice50%~80%
Number of Foreign Trading Staff5
Overseas Agent/BranchNo
New Products Launched in Last yearNo

Our Certifications, Standards & Industry Recognition

Cooperated with Fortune 500No

Product Q&A

Q:Q:Can you send samples?
A:
A:Of course, we can send samples to all parts of the world.
Q:Q:What are the shipping ports?
A:
A:Under normal circumstances, we ship from Tianjin, Qingdao ports, you can choose other ports according to your needs.
Q:Q:What are the certifications for your products?
A:
A:We have ISO 9001, SGS, EWC and other certifications.
Q:Q:How long does your delivery time take?
A:
A:In general, our delivery time is within 7-15 days, and may be delayed if the demand is extremely large or special circumstances occur.
Q:Q:Can I go to your factory to visit?
A:
A:Of course, we welcome customers from all over the world to visit our factory.

Send Inquiry

*To:Jiangsu Zunxiang International Trade Co., Ltd.
*Content:
0/4000

Supplier replies will be sent to your registered email

You may also like

Oxidation Resistant High Temp Inconel Alloy Pipe
Made-in-China.com